🧪 Want to create your own conductive ink using RGO? Here’s a simple lab-scale recipe:
✅ Ingredients:
-
50 mg reduced graphene oxide (dry or from dispersion)
-
5 mL water or isopropyl alcohol (IPA)
-
1–2 drops surfactant (e.g., Triton X-100)
-
Optional: small amount of PVP or binder for coating adhesion
⚙️ Method:
-
Mix RGO and solvent in beaker.
-
Add surfactant and stir 5 min.
-
Ultrasonicate for 10 min (optional but recommended).
-
Use immediately by brush, dip, or spray.
🖨️ Use Cases
-
Brush-on circuit repairs
-
Low-cost EMI prototypes
-
Substrate testing (plastic, paper, glass)